Arcam announces CoCr option for its Q10plus Additive Manufacturing system

Arcam announces CoCr option for its Q10plus AM system

Arcam’s Q10plus can now process CoCr powders

Sweden’s Arcam AB has announced that its latest Q10plus Electron Beam Melting (EBM) Additive Manufacturing system can now process Cobalt Chrome (CoCr) metal powders. The company will be displaying the Q10plus at the formnext exhibition in Frankfurt, November 15-18, 2016.

CoCr is, together with titanium, the prime material for the orthopaedic industry and it is also a commonly used material in the aerospace industry. The availability of CoCr on the Arcam Q10plus system will now allow users in the orthopaedic market to take full advantage of the production capabilities of Arcam’s EBM technology.

Arcam states that its CoCr process provides parts with high resolution, production level productivity and impeccable material properties. The company added that the process has also been supported by an animal study undertaken at Gothenburg University, showing bone interaction with CoCr. Parts made by the new process will also be on display at Arcam’s exhibition stand in Hall 3/F20.

The newly released Arcam Q10plus is the latest iteration of Arcam’s EBM technology. The system offers a range of key features including the company’s xQam™ X-ray based detection system for automatic calibration and improved beam control, along with its new EBM Control 5.0 software platform to add functionality for more efficient and accurate beam control as well as new melt strategies, improving build speed and precision.

www.arcam.com

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap