Simufact to launch process simulation software solution for metal Additive Manufacturing

News
September 29, 2016
simufact

Simufact Engineering GmbH, a MSC Software company based in Hamburg, Germany, has announced the launch of Simufact Additive, a new software solution for the simulation of metal Additive Manufacturing processes.

Simufact Additive is said to be a powerful and scalable process simulation environment for ‘right first time’ optimisation of laser powder bed fusion processes. Features include simulation of all the key AM process steps starting with ‘printing’ of the part followed by heat treatment, cutting the part off the build plate and removal of support structures, plus heat and pressure combined processes.

The company stated that initial release of Simufact Additive will predict the final distortion and residual stresses of the metal parts. The modelling is carried out using CAD data in an innovative graphical user interface (GUI) environment aligned with the real process work flow.

Simufact Additive offers an intuitive approach which starts with defining the general process by determining the part and support components. It continues through to definition of manufacturing parameters up to the analysis settings and ultimate results. The software helps to compensate the distortion, minimize residual stresses and optimise the process parameters.

“Today, companies employing AM technology for printing metal parts have to cope with failure in their production processes and the high knock on costs associated with this,” stated Michael Wohlmuth, Simufact`s CEO. “Simufact Additive is an important tool which will help these companies get it ‘right first time’, by regularly running simulations prior to production.”

The concept behind the software is that it lays the foundation for a wide variability and scalability through different levels of details. This includes both a fast mechanical method for the prediction of distortion and residual stresses up to a fully thermo-mechanically coupled transient analysis. This will determine the temperature history and derived properties such as the microstructure. The properties of the final part are available for subsequent structural simulations.

Simufact stated that Renishaw plc is the first AM machine vendor to collaborate with the company. The aim is a fully simulation based optimisation leading to the best quality build file. Initially, Renishaw’s QuantAM build preparation software will be coupled with Simufact process simulation software and enable data exchange using QuantAM’s open API (application programming interface). The next step is to automatically set-up a simulation based on the build information and in return to display the simulation results in Renishaw’s QuantAM build preparation software. The first results of this collaboration will be published and showcased at Formnext 2016, November 15-18, Frankfurt, Germany.

www.simufact.com/additive

News
September 29, 2016

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap