Cooksongold announces distribution partnership with Materialise

Cooksongold, based in Birmingham, UK, has announced a partnership with Materialise NV, Leuven, Belgium, that will lead to the distribution of its Cooksongold Precious M 080 metal Additive Manufacturing system with Materialise’s Magics and Build Processor software.

precious-m-080

Cooksongold, part of the Heimerle + Meule Group, has a long history of manufacturing precious metal products for the jewellery and watchmaking industries. In collaboration with EOS, Cooksongold distributes the Precious M 080 metal Additive Manufacturing system. This technology allows users to create complex jewellery and watch components that were previously considered impossible or too time-consuming to be commercially viable.

Cooksongold provides a complete turnkey solution by producing a range of advanced precious metal powders in 18k gold, 950 platinum and 925 silver, which have been developed especially for optimum use with the Precious M 080.

Following the new agreement with Materialise, the software package will allow users to easily prepare data, generate support, communicate their files to the metal AM machine, and overview all installed machinery. Users will also be able to handle large files, produce complex parts, streamline their production process and track their manufactured parts.

www.cooksongold-emanufacturing.com 

www.software.materialise.com   

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap