Cancer patient receives Additive Manufactured ribs in world first surgery

A Spanish cancer patient has received an Additive Manufactured titanium sternum and rib cage, in what is stated to be a world-first operation. The design and manufacture of the implant was the result of international collaboration between the patient’s surgical team based at Salamanca University Hospital, Spain, and Anatomics, a medical device company based in Melbourne, Australia, along with CSIRO’s 3D printing facility, Lab 22, in Clayton, Australia.

rib-cage-1

The 54 year old patient, suffering from a chest wall sarcoma, required his sternum and a portion of his rib cage to be replaced. This part of the chest is stated to be difficult to recreate with prosthetics due to the complex geometry and individual design required for each patient. The surgical team identified Additive Manufacturing as the best option for a fully customisable sternum and rib cage.

The surgical team, Dr José Aranda, Dr Marcelo Jimene and Dr Gonzalo Varela from Salamanca University Hospital, knew the surgery would be difficult due to the complicated geometries involved in the chest cavity. “We thought, maybe we could create a new type of implant that we could fully customise to replicate the intricate structures of the sternum and ribs,” stated Dr Aranda. “We wanted to provide a safer option for our patient, and improve their recovery post-surgery.”

The implant was designed and manufactured by medical device company Anatomics, who utilised the CSIRO’s 3D printing facility, Lab 22. After assessing the complexity of the requirements, Anatomics CEO Andrew Batty said the solution lay in metallic 3D printing.

“We wanted to 3D print the implant from titanium because of its complex geometry and design,” Batty stated. “While titanium implants have previously been used in chest surgery, designs have not considered the issues surrounding long term fixation. Flat and plate implants rely on screws for rigid fixation that may come loose over time. This can increase the risk of complications and the possibility of reoperation.”

Through high resolution CT data, the Anatomics team were able to create a 3D reconstruction of the chest wall and tumour, allowing the surgeons to plan and accurately define resection margins. “From this, we were able to design an implant with a rigid sternal core and semi-flexible titanium rods to act as prosthetic ribs attached to the sternum,” Batty added.

Working with experts at CSIRO’s 3D printing facility Lab 22, the team then manufactured the implant out of surgical grade titanium alloy using an Arcam EBM system. Once the prosthesis was complete it was couriered to Spain and implanted into the patient.

“The operation was very successful,” Dr Aranda stated. “Thanks to 3D printing technology and a unique resection template, we were able to create a body part that was fully customised and fitted like a glove.”

www.anatomics.com   

www.csiro.au   

Useful links

To submit news and articles for publication on Metal Additive Manufacturing email us at [email protected] 

Go to the Metal-AM homepage | View all news | Subscribe to our free e-newsletter

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap