Airbus A320neo passenger jet takes off with Additive Manufactured parts in LEAP jet engines

A next-generation A320neo Airbus passenger jet, powered by twin LEAP jet engines with Additive Manufactured parts, is reported to have completed its maiden flight on May 19, 2015, in Toulouse, France.

The LEAP is the first engine equipped with 19 3D-printed fuel nozzles, as well as parts made from high performance ceramics that make it 15% more fuel efficient than comparable engines built by CFM International, the 50/50 joint-venture between GE Aviation and France’s Safran (Snecma) that designed the engine.

a320neo

An Airbus A320neo powered by a pair of LEAP-1A engines took a maiden flight on May 19 in Toulouse, France. Image credit: Airbus 

“Today, we are celebrating the next step in our very successful journey with Airbus, a journey that goes back nearly 35 years to the very launch of the A320 program,” stated Jean-Paul Ebanga, President and CEO of CFM.

The two engines used for the four and a half hour flight were the LEAP-1A, developed specifically for the Airbus jet. Airbus picked the LEAP for the A320neo in 2010. Since then, CFM has received more than 2,500 orders and commitments for the LEAP-1A engine, representing 55% of A320neo orders to date.

fig10

There are 19 of these AM fuel nozzles in

each of GE’s new LEAP passenger jet

engines

CFM International also designed the LEAP-1B for Boeing’s 737 MAX aircraft, and LEAP-1C for Comac’s C919 planes.  With a running tally of 8,900 orders valued around $115 billion (US list price), the LEAP is the bestselling engine in GE Aviation’s history.

CFM has said it was “on track” to receive joint US Federal Aviation Administration and European Aviation Safety Agency certification. The first LEAP is scheduled to enter service in 2016.

There are currently more than 30 LEAP engines (all three models) in final assembly or going through tests at GE and Snecma testing facilities in Peebles, Ohio, Victorville, Cal., and elsewhere in Europe and around the world. The testing program has logged a total of more than 3,660 certification test hours and 5,460 test cycles.

The FAA recently certified the first 3D-printed part for a GE jet engine – a casing that houses the compressor inlet temperature sensor inside the GE90 jet engine.

www.ge.com  


Subscribe to our FREE e-newsletter

Useful links:  News | Articles | Introduction to metal Additive Manufacturing


 

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap