New GE plant to assemble world’s first passenger jet engine with additive manufactured fuel nozzles

GE Aviation has announced it will open a new $100 million assembly plant in Indiana, USA, to build the world’s first passenger jet engine with fuel nozzles produced by Additive Manufacturing (3D Printing) technology. The company stated that additively manufactured fuel nozzles will be used in its new LEAP engine, a joint venture between GE and France’s Snecma, which will enter service in 2016 and already has 6000 confirmed orders valued at $78 billion.

leap-nozzle

GE will use 19 of these AM fuel nozzles in each

LEAP engine

The new plant will be based in Lafayette, Indiana, and will employ around 200 people by 2020. GE will operate an advanced assembly line equipped with automated vision inspection systems, radio frequency parts management and other new technologies designed to improve production.

Each LEAP engine has 19 additively manufactured fuel nozzles which are five times more durable than the previous model. Additive Manufacturing allowed engineers to use a simpler design that reduced the number of brazes and welds from 25 to just five.

GE also reported that the engine incorporates a number of next-generation materials including heat-resistant ceramic matrix composites (CMCs) and breakthrough carbon fibre fan blades woven in all three dimensions at once. The CMC parts help with weight and heat management. They are two-thirds lighter than the metal equivalent and can operate at temperatures 20% higher than their metallic counterpart, at levels when most alloys grow soft.

leap-engine

The new LEAP engine suspended on a test rig

“When you start thinking about design, the weight savings multiplier effect is much more than three to one,” stated Michael Kauffman, GE Aviation Manufacturing Executive. “Your nickel alloy turbine disc does not have to be so beefy to carry all those light blades, and you can slim down the bearings and other parts too because of a smaller centrifugal force. It’s just basic physics.”

The new technologies allowed the design team to cut the engine’s weight by hundreds of pounds compared to the same size engine built using metal parts, increase the internal temperature and make it more efficient. “We are pushing ahead in materials technology, which gives us the ability to make jet engines lighter, run them hotter, and cool them less,” Kauffman added. “As result, we can make the engines, and the planes they’ll power, more efficient and cheaper to operate.”

leap-test

A LEAP 1-A engine is powering through an icing test 

The LEAP engine has benefited from GE’s $1 billion annual investment in jet propulsion R&D. Scientists at GE Global Research have spent the last two decades developing some of the most advanced parts of the new engine, including CMCs, Additive Manufacturing methods and controls systems.

www.ge.com

Useful links

To submit news and articles for publication on Metal Additive Manufacturing email us at [email protected]

Metal-AM homepage | Latest News | Subscribe to our free e-newsletter

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap