Shenyuan New Materials plans $4.5M EIGA titanium powder expansion

Shenyuan New Materials Technology (Hebi) Co., Ltd., located in Hebi, China, is reported to be expanding its manufacturing operations with an investment of RMB 30 million (approx. $4.5 million) in titanium and titanium alloy powder production. The project has entered the environmental approval process, with a proposed approval notice published by the Hebi Municipal Ecology and Environment Bureau on October 10, 2026.

According to the environmental impact assessment notice, the project will be located in an existing factory building at the Haili Magnesium Alloy Lightweight Equipment Industrial Park in the Hebi Economic and Technological Development Zone.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

The proposed facility will use Electrode Induction Melting Gas Atomisation (EIGA) technology to produce metal powders from titanium and titanium alloy electrode rods. The planned equipment includes an EIGA powder production system, air classifier, two-stage cyclone powder collector, rotary vibrating screen and double-cone mixer, together with associated surface treatment, inspection and packaging equipment.

EIGA is a crucible-free powder production process in which metal electrodes are melted using induction heating before the molten material is atomised using high-pressure inert gas. The process is used to produce spherical powders from reactive metals, including titanium alloys, for applications such as Additive Manufacturing.

The environmental assessment outlines measures to control dust generated during sandblasting and shot blasting, including cyclone separation and explosion-proof cartridge filtration. It also addresses wastewater management, equipment noise and solid waste disposal.

The published notice does not specify the facility’s planned annual powder production capacity or a commissioning date.

sthjj.hebi.gov.cn

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap