PSI scales up boron nitride coating process for 316L powders

MaterialsNews
June 10, 2026
PSI identified a fluidised bed reactor process as the most effective coating route (Courtesy Phoenix Scientific Industries)
PSI identified a fluidised bed reactor process as the most effective coating route (Courtesy Phoenix Scientific Industries)

Phoenix Scientific Industries Ltd (PSI), Hailsham, East Sussex, UK, has reported the successful development and scale-up of a process for coating 316L stainless steel powders with boron nitride nanoparticles for Additive Manufacturing applications.

According to PSI, its work addresses a longstanding challenge in powder engineering: achieving the uniform dispersion and application of nanoparticles onto metal powder surfaces at an industrially relevant scale. Nanoparticles have attracted interest for their potential to modify material properties and processing behaviour, but their tendency to form agglomerates has limited wider industrial adoption.

The company explained that initial investigations found commercially available boron nitride nanopowder exhibited significant agglomeration, requiring the development of specialised pre-processing methods prior to coating.

Several preparation routes were evaluated. PSI reported that low-energy ball milling increased agglomeration rather than reducing it, producing larger particle clusters. More promising results were achieved using a solution-based dispersion approach that combined controlled stirring and liquid-media processing. This reportedly reduced agglomerate sizes to approximately 1–2 µm and enabled subsequent coating operations.

A range of coating technologies was then assessed. While alternative methods provided useful process data, PSI stated that many resulted in uneven coatings or the formation of separate nanoparticle clusters rather than effective adhesion to the powder surface.

The company ultimately identified a fluidised bed reactor (FBR) process as the most effective coating route. By optimising gas flow, nanoparticle injection and fluidisation conditions, PSI reported achieving a uniform boron nitride coating on 316L stainless steel powder particles. Optical microscopy and scanning electron microscopy (SEM) analyses were said to confirm the presence of the coating layer through changes in particle surface appearance and reflectivity.

PSI also highlighted the successful scale-up of the process from laboratory to industrial production. Using a larger retort system, the company produced two 20 kg batches of coated powder while maintaining fluidisation behaviour, nanoparticle delivery and coating quality comparable to laboratory trials.

The company reported that its technology could support the development of advanced powder systems, including oxide dispersion-strengthened (ODS) alloys, high-temperature materials and wear-resistant components. PSI added that further work will focus on Laser Beam Powder Bed Fusion (PBF-LB) Additive Manufacturing and mechanical property evaluation of components produced using the coated powders.

www.psiltd.co.uk

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
MaterialsNews
June 10, 2026

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap