Innospace commercialises support-free titanium AM process

Dome-shaped titanium high-pressure tank produced using a support-free Additive Manufacturing process (Courtesy Innospace)
Dome-shaped titanium high-pressure tank produced using a support-free Additive Manufacturing process (Courtesy Innospace)

Innospace, headquartered in Sejong, South Korea, claims that it has become the first in South Korea to commercialise an advanced metal Additive Manufacturing process that produces high-precision titanium components without support structures.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

The technology is reported to enable the efficient production of complex curved structures, such as spherical and dome-shaped components, reducing both time and cost.

“The advanced metal manufacturing sector is characterised by high technological entry barriers and stringent quality verification standards, making it a strategically important field where securing core technologies directly impacts scalability and profitability,” said Soojong Kim, Founder and CEO of Innospace.

The company expects it to change manufacturing approaches for key aerospace and defence components, including satellite propellant tanks. The development extends the company’s advanced technological capabilities accumulated through the development of its ‘HANBIT’ launch vehicle into commercial manufacturing applications.

“Building on our Additive Manufacturing capabilities developed through launch vehicle programmes, we will accelerate expansion into high-value markets, including aerospace, defence, and satellite structures, and strengthen our competitive position in the global market,” added Kim.

Comparison of conventional additive manufacturing processes (left) and advanced support-free additive manufacturing processes (right) (Courtesy Innospace)
Comparison of conventional additive manufacturing processes (left) and advanced support-free additive manufacturing processes (right) (Courtesy Innospace)

In conventional metal AM processes, internal support structures are typically required to prevent deformation during fabrication. This results in increased post-processing, longer production times, and limitations in design freedom. Innospace states that it has achieved product quality and structural stability without support structures by applying advanced process control technologies, even within standard Laser Beam Powder Bed Fusion (PBF-LB) environments. The company also addressed key technical challenges associated with titanium materials, which are prone to thermal distortion and require highly sophisticated process control.

Innospace supplied high-precision components produced using this process to a domestic aerospace company in December last year, demonstrating real-world application and validation. According to Innospace, the technology reduced manufacturing time by a factor of 2.5 and cut costs by up to 40% by significantly reducing post-processing steps.

Enhanced design freedom also enables lightweighting and performance optimisation, reportedly allowing the company to meet aerospace transportation and defence requirements more consistently.

www.innospc.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap