Atherton launches additively manufactured titanium cranks

ApplicationsNews
March 10, 2026
Atherton's additively manufactured cranks feature an internal structure that balances strength and weight (Courtesy Atherton Bikes)
Atherton’s additively manufactured cranks feature an internal structure that balances strength and weight (Courtesy Atherton Bikes)

Atherton Bikes, based in Machynlleth, Wales, UK, has expanded its range of additively manufactured products with the introduction of the A.GR.TI crankset, produced from aerospace-grade titanium.

“Cranks are fundamentally simple components: a lever connecting your pedals to a chainring and spindle,” stated Scott Aisthorpe, Design Engineer. “But while it’s simple, they’re heavily loaded and sit directly in harm’s way, with endless opportunity for refinement and optimisation. And that’s exactly what we’ve done, from structural performance to ground clear and fit.”

The crankset functions as a three-piece system, with two separate titanium crank arms and an aluminium spindle (Courtesy Atherton Bikes)
The crankset functions as a three-piece system, with two separate titanium crank arms and an aluminium spindle (Courtesy Atherton Bikes)

The new crank arms feature an internal structure that balances strength and weight. The design combines internal engineering features with a durable exterior intended for use in demanding mountain biking conditions. The inside features ribs with hollow pockets, a lightweighting design choice, while the tip around the pedal thread is solid to offer increased durability. Likewise, the front and rear faces are closed to shed mud.

The crankset functions as a three-piece system, with two separate crank arms and an aluminium spindle, allowing it to be interchanged between trail and downhill bikes. The system’s self-extracting bolt is detachable at home, allowing users to disconnect the crank’s arms from either side of the spindle.

According to the company, the crankset has been laboratory tested and evaluated under EFBE and ISO Category 5 conditions using the same set of cranks, which reportedly reached the maximum load on the EFBE jump-load test rig.

The A.GR.TI cranks are available in multiple lengths and with three surface finishes – raw, burnished and tumbled – allowing riders to configure the components to suit their preferences.

www.athertonbikes.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
ApplicationsNews
March 10, 2026

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap