AddMamBa advances recycled construction steel for AM facade brackets

MaterialsNewsResearch
February 13, 2026
AddMamBa investigates how CO₂ emissions and resource consumption in construction can be reduced (Courtesy RWTH Aachen University Chair Digital Additive Production)
AddMamBa investigates how CO₂ emissions and resource consumption in construction can be reduced (Courtesy RWTH Aachen University Chair Digital Additive Production)

AddMamBa, the BMWE-funded research project at the RWTH Aachen University Chair Digital Additive Production (DAP), is investigating how CO₂ emissions and resource consumption in the construction sector can be reduced with a focus on optimised, additively manufactured, and reusable facade brackets made from recycled steel. These components enable targeted reductions in material usage as well as thermal weak points.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

According to the UN Global Construction Report 2024/25, approximately 34% of global energy-related CO₂ emissions and 32% of worldwide energy consumption are attributable to the construction sector. As a result, strategies focused on resource efficiency, circular economy approaches, and the reuse of construction materials are gaining importance in both research and industrial practice. Additive Manufacturing is regarded as a key enabling technology for economically utilising secondary raw materials while producing functionally optimised, material-efficient components.

From construction waste to metal powder for Additive Manufacturing

Concrete rubble processing at a recycling facility (left); steel scrap collection using a hydraulic magnet (right) (Courtesy Paul Kamrath Ingenieurrückbau GmbH)
Concrete rubble processing at a recycling facility (left); steel scrap collection using a hydraulic magnet (right) (Courtesy Paul Kamrath Ingenieurrückbau GmbH)

The research focuses on two types of components: facade brackets for ventilated facade systems (VHF) and connectors for load-bearing structures. As part of the project, these components are manufactured using Laser Beam Powder Bed Fusion (PBF-LB). The required metal powder is produced from steel scrap, which is first sorted by age, grade (e.g. reinforcing steel or structural beams), and condition, then analysed for its chemical composition. The powder is then produced using gas atomisation (VIGA). In a further step, the powder is sieved to obtain a particle size fraction of 15-45 micrometres that ensures a uniform layer build-up in the PBF-LB process.

This approach is intended to ensure that the recycled steel meets the quality requirements for load-bearing facade components.

Optimised, circular, and additively manufactured

Workflow for the development of the topology-optimised facade bracket (Courtesy RWTH STB)
Workflow for the development of the topology-optimised facade bracket (Courtesy RWTH STB)

Due to the nature of the manufacturing process, facade connections can be individually adapted to building geometry, substructure configuration, and regional requirements, without additional costs for dedicated tools or moulds. Topology optimisation enables load-path-oriented material distribution, improving mechanical load-bearing performance while simultaneously reducing thermal weak points such as thermal bridges.

A digital planning tool developed within the project helps users select suitable bracket solutions. “After entering relevant building and facade data as well as the substructure configuration, the tool provides a robust basis for identifying the most suitable bracket in each case,” explained researcher Joana Schulte. The tool takes into account relevant standards, in particular DIN EN 1991-1-4/NA.

Further development and optimisation of connection elements: variants of the sigma node, with an overall view shown above and the corresponding sectional view shown below (Courtesy RWTH DAP)
Further development and optimisation of connection elements: variants of the sigma node, with an overall view shown above and the corresponding sectional view shown below (Courtesy RWTH DAP)

In addition, the project applies a life-cycle-oriented design approach: the components are designed to be demountable, separable by material type, and reusable.

Outlook and life cycle assessment

As part of a Life Cycle Assessment (LCA) conducted in accordance with DIN EN 15804, initial calculations based on conservative electricity-mix scenarios indicate a Global Warming Potential of 23.8-33.5 kg CO₂ equivalents per kilogram of component (2030), with a further downward trend expected as the share of renewable energy increases, according to the project team.

The analysis also shows that offsetting the higher manufacturing-related emissions, associated with the developed approach, through operational savings is most pronounced in buildings with conventional gas heating systems. When combined with modern heat pump systems, this effect is less significant.

For this reason, the circular economy aspect of the project is particularly important. In experimental trials, approximately 60% of usable metal powder was recovered from the processed steel scrap (30 kg of powder from 50 kg of scrap). This demonstrates that recycled steel can, in principle, be qualified for AM of functionally relevant facade connections.

The material-pure disassembly of newly developed and further optimised brackets and connector solutions provides an additional significant contribution toward closed material cycles.

Industry and practice

The research team stated that, for architectural firms, engineering consultancies, facade contractors, and manufacturers of connection elements, the project offers valuable insights. Additive Manufacturing not only enables functionally optimised geometries but also unlocks the potential to convert steel scrap into high-quality components, thereby helping to close material loops in the construction sector.

The project has developed an application pathway for making secondary materials usable within the AM process chain for the construction sector. This outcome is also relevant for powder manufacturers and AM users.

The project consortium is as follows:

  • Paul Kamrath Ingenieurrückbau GmbH
  • RSB Rudolstädter Systembau GmbH
  • Laser Melting Innovations GmbH
  • RWTH Aachen University
    • Chair Digital Additive Production (DAP)
    • Institute of Steel Construction – Sustainable Metal Building Envelopes Teaching and Research Area (MLB)
    • Chair for Steel and Lightweight Construction (STB)

The research and development project “Additive Manufacturing of 3D Connection Elements in Construction (AddMamBa)” is funded by the German Federal Ministry for Economic Affairs and Energy (BMWE) under the Lightweight Technology Transfer Program (funding code 03LB3019B) and is managed by Project Management Jülich (PTJ).

dap-aachen.de

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
MaterialsNewsResearch
February 13, 2026

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap