LLNL links laser scan speed to atomic-scale control in High-Entropy Alloys

MaterialsNewsResearch
February 11, 2026
Artist’s rendering of LLNL's additively manufactured HEA, developed using a laser scan speed adjustment method (Courtesy Daniel Herchek/LLNL)
Artist’s rendering of LLNL’s additively manufactured HEA, developed using a laser scan speed adjustment method (Courtesy Daniel Herchek/LLNL)

In a new study published in Advanced Materials, researchers from Lawrence Livermore National Laboratory (LLNL) and collaborators from several universities have demonstrated a method to guide the settling of atoms as a metal solidifies during Additive Manufacturing.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

By adjusting the laser speed in a High-Entropy Alloy (HEA), the team reportedly controlled the material’s properties directly at the atomic scale.

In ‘Unravelling Microstructure Selection in an Additively Manufactured Eutectic High-Entropy Alloy’, the researchers combined thermodynamic modelling and molecular dynamics to simulate the Additive Manufacturing of HEAs in order to determine how the cooling rate impacts the internal structures.

“By increasing the laser speed, the cooling rate increases and, as the material cools down faster, it has less time to rearrange into a low energy configuration,” explained Thomas Voisin, Deputy Group Lead. “This freezes the material in a non-equilibrium state, which can be used to tune atomic structures and resulting mechanical properties.”

Fast cooling yields a very strong but more brittle alloy; slower cooling yields more flexible, balanced structures. By adjusting the laser speed, the researchers were able to create this range of properties in the single HEA material investigated.

“We are now at a place where we can effectively design new materials that take full advantage of the Additive Manufacturing features like the very rapid cooling rate,” added Voisin.

The researchers have stated that this development could enable the use of Additive Manufacturing as a platform for producing metals with specially engineered properties.

The paper is available here.

llnl.gov

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
MaterialsNewsResearch
February 11, 2026

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap