Scandium Canada signs MoU with Gränges PM for aluminium-scandium alloys

MaterialsNews
November 12, 2025
Scandium Canada will explore the integration of its proprietary alloys into Gränges Powder Metallurgy’s product portfolio (Courtesy Scandium Canada)
Scandium Canada will explore the integration of its proprietary alloys into Gränges Powder Metallurgy’s product portfolio (Courtesy Scandium Canada)

Scandium Canada Ltd, headquartered in Montreal, has entered into a Memorandum of Understanding (MoU) with Gränges Powder Metallurgy (GPM), Velbert, Germany, under which the companies will explore the integration of Scandium Canada’s proprietary Sc-modified AA535 and AA7075 aluminium-scandium alloys into GPM’s offering.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

According to Dr Luc Duchesne, Head of Scandium+ division and Chief Science Officer, Scandium Canada’s proprietary alloys directly address the critical need for high-strength and lightweight metals for Additive Manufacturing in sectors such as aerospace, automotive, and advanced manufacturing. He went on to state this MoU demonstrates Scandium Canada’s efforts to cooperate at different levels of the scandium value chain to accelerate the uptake of its alloys.

Scandium Canada also stated it has received Productique Québec’s report on their analysis of the best-case uses of its patent-pending aluminium-scandium alloys. The Productique study identified thirteen target alloy applications and relevant organisations for specific industrial users, including welding wires, aircraft ducting, and heat exchangers. Each of the thirteen applications is attached to particular commercial stakeholders that could benefit from Scandium Canada’s alloys.

Guy Bourassa, CEO of Scandium Canada, stated that Productique Québec’s work provided a strong validation of the commercial potential of its alloys. He added that the company is encouraged that its technical assessment confirmed the applicability of their alloys based on their demonstrated laboratory properties but also identified new uses that extend beyond their initial scope.

The company has secured in-kind support from Canada’s Industrial Research Assistance Program (IRAP) to collaborate with experts from the Additive Manufacturing Division of the National Research Council of Canada (NRC). This partnership will focus on identifying new commercial applications and pathways for the company’s alloys.

Scandium Canada’s AA535 and AA7075 alloys and their method of fabrication were developed and tested in collaboration with McMaster University, Hamilton, Canada, and are protected by a newly filed international patent application under the Patent Cooperation Treaty (PCT).

www.granges.com

www.scandium-canada.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
MaterialsNews
November 12, 2025

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap