MBDA achieves missile system flight with complex multifunctional AM part

ApplicationsNews
October 21, 2025
MBDA’s successful flight test confirmed that its AM component delivers the required functionality and performance in real operational conditions (Courtesy MBDA)
MBDA’s successful flight test confirmed that its AM component delivers the required functionality and performance in real operational conditions (Courtesy MBDA)

MBDA, headquartered in Le Plessis-Robinson, France, has additively manufactured a complex multifunctional component used to house vital electronic equipment in next-generation missile systems. Believed to be the first use of AM for this application, the company reported that the missile recently concluded its successful maiden flight.

Produced in titanium alloy using Laser Beam Powder Bed Fusion (PBF-LB), the innovative component provides a range of new functionalities in addition to its essential structural role. Additive Manufacturing has enabled the integration of electronic boards directly into the body, optimising assembly and improving performance.

Another significant benefit of using Additive Manufacturing, highlighted by MBDA, is its capability to optimise thermal management. By creating a double-skin structure, the design provides thermal insulation, reducing internal temperature rise by up to 70%. This approach also allows MBDA to dramatically reduce mass and optimise the component’s volume.

The design and development of the component resulted from collaboration between MBDA’s Mechanical Engineering and Industrial departments, underpinned by advanced digital simulation tools tailored for Additive Manufacturing processes. More than fifty prototypes were produced and underwent comprehensive tests to validate fatigue resistance, thermomechanical stability, and firing performance – critical elements for military applications.

The next phase of the project consists of part qualification and transition to series production, said to be enabled by a dedicated industrial roadmap focused on AM. This strategy includes developing robust supply chains and investing in new, larger, and more efficient AM machines.

www.mbda-systems.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
ApplicationsNews
October 21, 2025

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap