Synergy Additive Manufacturing secures Navy SBIR contract for titanium coating of helicopter components

ApplicationsNews
July 14, 2025
Synergy Additive Manufacturing LLC has been awarded a Phase I Small Business Innovation Research (SBIR) contract from the Naval Air Systems Command (NAVAIR) (Courtesy Synergy Additive Manufacturing)
Synergy Additive Manufacturing LLC has been awarded a Phase I Small Business Innovation Research (SBIR) contract from the Naval Air Systems Command (NAVAIR) (Courtesy Synergy Additive Manufacturing)

Synergy Additive Manufacturing LLC, based in Clinton Township, Michigan, USA, has been awarded a Phase I Small Business Innovation Research (SBIR) contract from the US Naval Air Systems Command (NAVAIR) to develop Extremely High-Speed Laser Cladding (EHLA) processes to enhance the performance of titanium cylinder bores used in essential helicopter components. The SBIR award supports the US Navy’s goal of extending the life of key aerospace systems while reducing costs and downtime associated with conventional overhaul methods.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

Under this programme, Synergy will develop processes and advance materials optimised for high-deposition and precision cladding on titanium alloys. The work will target rapid, distortion-free and defect-free cladding of cylinder bores while minimising material waste and extending the service life of performance-critical components.

“Synergy has been at the forefront of developing advanced laser processing technologies, including high-speed laser cladding,” said Aravind Jonnalagadda, CTO of Synergy Additive Manufacturing. “This SBIR award gives us the opportunity to advance innovative material solutions, processes, and equipment that will not only support the operational readiness of our defence forces but also enhance the competitiveness of the US manufacturing industry.”

synergyadditive.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
ApplicationsNews
July 14, 2025

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap