TEMISTh developing ultra-thin heat exchangers using copper Additive Manufacturing

ApplicationsNews
July 14, 2025
TEMISTh is researching the use of copper Additive Manufacturing to produce custom heat exchangers (Courtesy TEMISTh)
TEMISTh is researching the use of copper Additive Manufacturing to produce custom heat exchangers (Courtesy TEMISTh)

As electronic devices become smaller and their power densities increase, efficient heat dissipation is becoming more important to ensure reliability and performance, explains TEMISTh, based in Lambesc, France. To address these challenges, the company is researching the use of copper Additive Manufacturing to produce custom heat exchangers.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

Additive Manufacturing makes it possible to create heat sinks with complex geometries that are impossible to achieve using conventional processes, while maintaining minimal thickness. The technology is paving the way for customised heat exchangers tailored to the specific needs of each application.

The TEMISTh team is focusing on the design of thin copper heat sinks that are adapted to the space constraints of modern power converters. Using advanced numerical simulation tools, the researchers are working to optimise the shape, internal structure, and heat flow distribution to maximise cooling efficiency while limiting hydraulic pressure drop.

TEMISTh is combining computer-aided design (CAD) and thermal simulation to design more compact, higer performance thermal management solutions (Courtesy TEMISTh)
TEMISTh is combining computer-aided design (CAD) and thermal simulation to design more compact, higer performance thermal management solutions (Courtesy TEMISTh)

To validate the performance of these new heat sinks, TEMISTh is preparing to launch an experimental testing campaign. This will focus on measuring thermal resistance and pressure drop as a function of heat transfer fluid flow rate. The data collected will then be used to refine simulation models and further optimise the designs.

By combining computer-aided design, thermal simulation, Additive Manufacturing, and experimental characterisation, TEMISTh expects the results will pave the way for more compact, higher-performance devices that are better suited to the demands of future electronics.

temisth.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
ApplicationsNews
July 14, 2025

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap