Velta receives third US patent for titanium powder production process

MaterialsNews
June 3, 2025
Velta Holding has received a third US patent for its Velta Ti Process (Courtesy Velta Holding)
Velta Holding has received a third US patent for its Velta Ti Process (Courtesy Velta Holding)

Velta Holding US Inc, a titanium feedstock company operating in the USA and Ukraine, has received a third patent from the United States Patent and Trademark Office (USPTO) for its Velta Ti Process technology.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

This new patent underlines Velta’s ability to produce high-quality titanium dioxide (TiO₂) – a key intermediate used in furthering the production of titanium powder using the Velta Ti Process, along with marketable titanium-, iron-, calcium-, and nitrogen-based by-products.

“We’ve received three US patents – all during the full-scale war,” said Andriy Brodsky, president of Velta Holding. “Our group has remained committed to our strategy of vertical integration through innovation, including Additive Manufacturing and 3D printing. I believe Ukraine has strong scientific potential, and these patents from the USPTO make me feel confident.”

Since 2017, Ukrainian chemists and metallurgists at the Velta RD Titan R&D centre have been working to develop, improve, and patent a method for producing titanium metal powders and alloys via its Velta Ti Process. Velta Holding has invested over $7 million in this research.

Compared to conventional multi-stage production methods, the Ukrainian technology is said to be less energy-intensive, have a significantly reduced carbon footprint, and offer superior economic efficiency. The new method is also referred to as zero-waste, enabling the production of by-products used in coatings, polymers, paper, pigment, and metallurgy industries.

Since 2020, Velta Holding US has secured three US and three Ukrainian patents:

  • Production of titanium powders and premium alloys using metallothermic methods
  • An original high-temperature process for titanium oxide reduction in molten salts
  • A zero-waste process for the cost-effective production of high-quality TiO₂ and valuable by-products designed to make the technology environmentally safe and commercially viable

Velta Holding plans to scale up from semi-industrial powder production at its R&D facility to a fully operational plant that will produce titanium powders and finished products based on its technology.

velta.us

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
MaterialsNews
June 3, 2025

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap