ORNL demonstrates how Additive Manufacturing can accelerate automotive manufacturing

ApplicationsNews
June 2, 2025
Two near-net shape dies were additively manufactured at Lincoln Electric Additive Solutions (Courtesy Lincoln Electric)
Two near-net shape dies were additively manufactured at Lincoln Electric Additive Solutions (Courtesy Lincoln Electric)

Researchers at the US Department of Energy’s Oak Ridge National Laboratory (ORNL), based in Oak Ridge, Tennessee, have demonstrated that using Additive Manufacturing to produce metal molds can offer a faster, more cost-effective, and flexible way to produce large composite components for mass-produced vehicles.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

Using Wire Arc Additive Manufacturing (WAAM) – a wire-based Directed Energy Deposition (DED) technology – the ORNL team reduced the weight of the complex metal molds, enabling efficiencies that could accelerate the adoption of lightweight composite materials in the automotive sector.

The research team partnered with Collaborative Composites Solutions (CCS), operator of IACMI–The Composites Institute. They chose to additively manufacture a large battery enclosure mold, complete with intricate internal features.

The lower mold, on the left, and the upper mold are shown fully assembled (Courtesy ORNL)
The lower mold, on the left, and the upper mold are shown fully assembled (Courtesy ORNL)

The team applied a specialised toolpath design strategy to reduce weight while maintaining strength. The two near-net-shape dies were then additively manufactured from stainless steel ER410 wire at Lincoln Electric Additive Solutions.

Subsequent analysis confirmed that the lightweighted mold met structural performance requirements, validating the feasibility of Additive Manufacturing for high-performance production tooling.

“This kind of technology can help reindustrialise the US and boost its competitiveness by creating smarter, faster ways to build essential tools,” said lead researcher Andrzej Nycz with ORNL’s Manufacturing Robotics and Controls group. “It brings us closer to an automated, intelligent production process.”

The mold was installed on a Wabash MPI 150-ton hydraulic press at the University of Tennessee, Knoxville, Fibers and Composites Manufacturing Facility (Courtesy University of Tennessee, Knoxville)
The mold was installed on a Wabash MPI 150-ton hydraulic press at the University of Tennessee, Knoxville, Fibers and Composites Manufacturing Facility (Courtesy University of Tennessee, Knoxville)

AM also allows engineers to produce more complex mold geometries, such as internal heating channels, that would be difficult to achieve using conventional machining. “The more complex the shape, the more valuable Additive Manufacturing becomes,” Nycz added.

The project was funded by US DOE’s Advanced Materials and Manufacturing Technologies Office (AMMTO). Additional researchers who contributed to this project include John Unser from Composite Applications Group, Peter Wang from ORNL, and Jason Flamm and Jonathan Paul from Lincoln Electric Additive Solutions.

www.iacmi.org

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
ApplicationsNews
June 2, 2025

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap