PyroGenesis gains Boeing approved supplier status for its titanium Additive Manufacturing powder

PyroGenesis titanium metal powder as produced by its NexGen  plasma atomisation system (Courtesy PyroGenesis)
PyroGenesis titanium metal powder as produced by its NexGen plasma atomisation system (Courtesy PyroGenesis)

PyroGenesis Inc, headquartered in Montreal, Quebec, Canada, has received official confirmation of approved supplier status with Boeing. The company stated that its Ti64 ‘coarse’ metal powder, with a particle size that is within the range of 53-150 µm, has been qualified for use and added to Boeing’s qualified list of metal powders available for use in Additive Manufacturing.

“PyroGenesis is proud to achieve official supplier status with Boeing,” said P Peter Pascali, President and CEO of PyroGenesis. “The high standard of Ti64 metal powder produced at PyroGenesis Additive for Boeing is the result of years of groundbreaking design and engineering work that went into developing our NexGen™ plasma atomisation process.”

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

Massimo Dattilo, Vice-President of PyroGenesis Additive, added, “Our stated goal to produce some of the highest quality metal powders in the Additive Manufacturing industry required being assessed by the highest quality client under the toughest standards. Having received qualification of our “coarse” powder, we look forward to serving the needs of Boeing and its parts manufacturing and service centres with metal powder produced by PyroGenesis’ NexGen™ plasma atomisation system.”

PyroGenesis invented the plasma atomisation process and coined the term ‘plasma atomisation’ in its original patent. The company has created proprietary, patented and advanced plasma technologies that are being vetted and adopted by multiple multibillion-dollar industries in four key markets: iron ore pelletisation, aluminium, waste management, and Additive Manufacturing.

www.pyrogenesis.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap