Oerlikon launches MetcoMed brand with metal powders for medical Additive Manufacturing applications

MaterialsNews
May 13, 2025
Additively manufactured titanium knee tip base (Courtesy Oerlikon Metco)
Additively manufactured titanium knee tip base (Courtesy Oerlikon Metco)

Oerlikon Metco, headquartered in Winterthur, Switzerland, has launched its new MetcoMed brand with the release of two materials tailored for the Additive Manufacturing of medical components and implants. The new metal powders, MetcoMed Ti64 G23-C, a titanium alloy, and MetcoMed CoCrMo F75-A, a cobalt-chromium alloy, are now available through the company’s distribution network.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

MetcoMed Ti64 G23-C

Building on the established and industry-approved alloy for Additive Manufacturing, Oerlikon’s MetcoMed Ti64 G23-C is said to provide high load-bearing capacity, good ductility, excellent biocompatibility, and good corrosion resistance.

The material reportedly offers a tensile strength of over 1000 MPa at 10% elongation. It has been optimised for Laser Beam Powder Bed Fusion Additive Manufacturing technology and can function as a direct drop-in solution for most machine brands.

Additively manufactured titanium hip implant (Courtesy Oerlikon Metco)
Additively manufactured titanium hip implant (Courtesy Oerlikon Metco)

MetcoMed CoCrMo F75-A

Cobalt-chromium alloys are widely used for various orthopaedic and dental implants, with CoCrMo one of the most used alloys for tooth implants and total hip replacement due to its superior corrosion qualities, antibacterial properties, improved cell adhesion, and potential for reducing inflammation markers.

Oerlikon has developed and launched a CoCrMo material specifically for PBF-LB Additive Manufacturing, noting the material’s high strength, ductility, and biocompatibility. MetcoMed CoCrMo F75-A provides a reported tensile strength of 1050 MPa and 35% elongation despite its low carbon content (desirable for an implant material). The powder exhibits a particle size distribution that enables its use on most PBF-LB AM platforms.

www.oerlikon.com/metco

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
MaterialsNews
May 13, 2025

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap