Researchers analyse nickel-aluminium-bronze ‘chip-powders’ for Directed Energy Deposition feedstock

MaterialsNews
May 7, 2025
SEM image of the NAB grinding chips used as feedstock for comminution in this study (Courtesy Müller, Vinzenz, et al, Recycling nickel aluminium bronze grinding chips to feedstock for Directed Energy Deposition via impact whirl milling: Investigation on processability, microstructure and mechanical properties, Additive Manufacturing)
SEM image of the NAB grinding chips used as feedstock for comminution in this study (Courtesy Müller, Vinzenz, et al, Recycling nickel aluminium bronze grinding chips to feedstock for Directed Energy Deposition via impact whirl milling: Investigation on processability, microstructure and mechanical properties, Additive Manufacturing)

German researchers from the Fraunhofer Institute for Production Systems and Design Technology IPK, Berlin; Mecklenburger Metallguss GmbH, Waren; and Technische Universität Berlin have published a paper in Additive Manufacturing focused on the processability, microstructure and mechanical properties of nickel-aluminium-bronze (NAB) grinding chips – a by-product of ship propeller manufacturing – when recycled as feedstock for Directed Energy Deposition (DED) Additive Manufacturing. The paper compared the ‘chip-powders’ produced by the comminution processes ball milling and impact whirl milling, as well as re-melting via ultrasonic atomisation.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

The researchers characterise the materials via digital image analysis, standardised flowability tests, scanning electron microscopy (SEM) and energy-dispersive X-ray spectroscopy and compare the feedstock to conventional gas atomised powder. The specimens deposited via Directed Energy Deposition are then analysed for density, hardness and microstructure; tensile properties for vertical and horizontal build-up directions are also compared.

Tensile samples produced in horizontal and vertical specimen blocks (Courtesy Müller, Vinzenz, et al, Recycling nickel aluminium bronze grinding chips to feedstock for Directed Energy Deposition via impact whirl milling: Investigation on processability, microstructure and mechanical properties, Additive Manufacturing)
Tensile samples produced in horizontal and vertical specimen blocks (Courtesy Müller, Vinzenz, et al, Recycling nickel aluminium bronze grinding chips to feedstock for Directed Energy Deposition via impact whirl milling: Investigation on processability, microstructure and mechanical properties, Additive Manufacturing)

At elevated mill rotation speeds, the comminution with impact whirl milling produced rounded particles, favourable flow properties and particle size distribution, making them suitable for Additive Manufacturing. The microstructure exhibited characteristic martensitic phases due to the high cooling rates of the AM process. The presence of ceramic inclusions was observed in both the powder and on the tensile fracture surfaces, partly impairing the mechanical properties. However, specimens in the vertical build-up direction (Z) showed competitive tensile results, with 775 MPa in tensile strength, 455 MPa in yield strength and 12.6% elongation at break.

The researchers noted that these findings indicate that recycling of machining chips into Additive Manufacturing feedstock can be a viable option for reducing material costs and environmental impact.

‘Recycling nickel aluminium bronze grinding chips to feedstock for Directed Energy Deposition via impact whirl milling: Investigation on processability, microstructure and mechanical properties’ is available here.

www.ipk.fraunhofer.de

www.mecklenburger-metallguss.com

www.tu.berlin

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
MaterialsNews
May 7, 2025

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap