Researchers assess effect of scan strategies on structure-property relationship in PBF-EB processed 316L

MaterialsNewsResearch
April 17, 2025
Schematic representation of the melt track and solidification conditions for inward and outward scan path. Insets show the OM images of observed top surfaces of S-5 and S-7 with melt track corner features, along with the cumulative scan time vs. scan track number for each scan strategies, as extracted from the OBP file (Courtesy Tarafder, Prithwish, et al, ‘Assessing the effect of scan strategies on the structure-property relationship in electron beam powder bed fusion processed 316L stainless steel’, Materials & Design)
Schematic representation of the melt track and solidification conditions for inward and outward scan path. Insets show the OM images of observed top surfaces of S-5 and S-7 with melt track corner features, along with the cumulative scan time vs. scan track number for each scan strategies, as extracted from the OBP file (Courtesy Tarafder, Prithwish, et al, ‘Assessing the effect of scan strategies on the structure-property relationship in electron beam powder bed fusion processed 316L stainless steel’, Materials & Design)

Researchers from Linköping University, Sweden, have published a paper in Materials & Design focused on the impact of eight different scanning strategies on the structure-property relationship in 316L austenitic stainless steel after production by Electron Beam Powder Bed Fusion (PBF-EB) Additive Manufacturing.

The results showed that variation in localised microstructure is principally determined by the beam path length and the extent of melting-remelting cycles. Sporadic dislocation sub-structures were observed in scan strategies where thermal conditions were more turbulent than the reference raster scan; this led to different mechanical responses despite lower measured densities.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

Average yield strength and ultimate tensile strength surpassed the conventionally produced and subsequently annealed 316L and were noted as being very close to the standards set forward for nuclear applications. These results open up the possibility of using different scan strategies in a PBF-EB machine that can exploit the scan path design freedom and achieve localised microstructural and property differences.

The researchers fabricated a proof-of-concept scaled-down version of an industrial component with varying scan patterns at different areas and mechanically tested the resultant part to showcase the feasibility of the presented approach.

‘Assessing the effect of scan strategies on the structure-property relationship in electron beam powder bed fusion processed 316L stainless steel’ is available here.

www.liu.se

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
MaterialsNewsResearch
April 17, 2025

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap