Penn State researchers achieve breakthrough in multi-metal Additive Manufacturing

A blue and gold CT scan of a metal beam (Courtesy Penn State)
A blue and gold CT scan of a metal beam (Courtesy Penn State)

Researchers from Pennsylvania State University, based in University Park, Pennsylvania, USA, have used a new Additive Manufacturing method to produce a complex metal build fusing two metals together into a single structure, a process that was once only possible with welding.

Using multi-material Laser Beam Powder Bed Fusion (PBF-LB) and a newly acquired machine at Penn State’s Center for Innovative Materials Processing Through Direct Digital Deposition (CIMP-3D), the researchers manufactured a complex structure out of a blend of low-carbon stainless steel and bronze, which consists of 90% copper and 10% tin.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

“In a process called selective powder deposition, we can now melt multiple powdered metals in a single layer during the Additive Manufacturing process — and we were the first university in the US to do so,” said Jacklyn Griffis, a doctoral candidate in mechanical engineering and first author of the paper. “The fine powders are tens of microns in diameter, almost like flour. We can selectively deposit the powder with micron-level resolution, then melt it together with a laser.”

The researchers used an Aerosint selective powder deposition machine integrated into an existing 3D Systems ProX320 AM machine in the Systems for Hybrid-Additive Process Engineering (SHAPE) Lab at CIMP-3D. Griffis explained that a one-centimetre-tall metal part includes thousands of layers of metal powder and takes a few hours to build.

“We now have the processing technology to print these multi-material metal parts, as well as a way to monitor the melt pool and observe and address potential issues in real time,” said corresponding author Guha Manogharan, associate professor of mechanical engineering, head of the SHAPE Lab and co-director of CIMP-3D. “To do this, we produce a digital 3D rendering of the part through CT scans, which we use to look for pores, cracks at the interface or micron-scale defects.”

A close-up view of a build plate of test squares featuring the first sintered layer of three metals: stainless steel, Inconel and pure copper. The test squares demonstrated multi-material metal Additive Manufacturing using CIMP-3D's new selective powder deposition system (Courtesy SHAPE Lab, CIMP-3D and 3D Systems)
A close-up view of a build plate of test squares featuring the first sintered layer of three metals: stainless steel, Inconel and pure copper. The test squares demonstrated multi-material metal Additive Manufacturing using CIMP-3D’s new selective powder deposition system (Courtesy SHAPE Lab, CIMP-3D and 3D Systems)

In manufacturing two metals in a single powder simultaneously, researchers had to work through complex questions on processing conditions and part quality. In this paper, the researchers focus on analysing the build orientation of the part to understand what would change if the part were manufactured upright, flat or on its side.

“In our analysis, we connected the part’s build orientation to a number of observations about the structure, including defects like cracking and porosity, interfacial microstructures and the ways elements are diffused or blended across the interface,” Griffis said. “We then connected those printed defects to the part’s performance.”

Their finished structure is a complex shape known as a gyroid, which is used in applications such as heat exchangers and biomedical implants. The researchers chose the gyroid shape to demonstrate the capabilities of the new manufacturing process – only multi-material PBF-LB can create a multi-material gyroid shape.

“Penn State has always been a leader in metal Additive Manufacturing, but we now have the ability to manufacture complex multi-material parts, where we can not only make complex designs but control precisely where each material is placed,” Manogharan said. “In order to get to full production, we need to understand the causes for defects based on materials and manufacturing conditions to address the question of why the parts failed at the interfaces.”

In future studies, the researchers will use an in-process monitoring system to transform the Additive Manufacturing method into a more robust, production-ready method. They also plan to incorporate other metal alloys into multi-material PBF-LB, such as Inconel and copper.

The full paper is available here.

www.psu.edu

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap