Trumpf qualifies 6K Additive’s titanium powder on TruPrint Additive Manufacturing machines

MaterialsNews
April 2, 2025
Qualification adds powder made from sustainable feedstock sources to Trumpf’s qualified partners (Courtesy 6K Additive)
Qualification adds powder made from sustainable feedstock sources to Trumpf’s qualified partners (Courtesy 6K Additive)

Trumpf, based in Ditzingen, Germany, has qualified titanium metal powder from 6K Additive, a division of 6K, based in North Andover, Massachusetts, USA, for use in its TruPrint Additive Manufacturing machines. Titanium Ti-6Al-4V is a high-strength, low-density alloy known for its excellent corrosion resistance. The powder’s biocompatible properties make it ideal for medical implants and applications in aerospace, automotive, and industrial sectors.

ADVERTISE WITH METAL AM
REACH ENGINEERS, DECISION-MAKERS AND INDUSTRY LEADERS SHAPING TECHNOLOGY ADOPTION
Request a Media Pack

“At Trumpf we are dedicated to making our customer’s experience with our TruPrint systems deliver the highest level of performance and this includes the powder they use for their metal parts,” said Dennis Pede, Material engineer and scientist at Trumpf. “TruPrint systems are open systems, allowing our customers to use the powder of their choice. However, for optimal process conditions and material properties, we recommend suitable material powders and work closely with our partners. Additionally, more and more our customers are asking us for metrics on the environmental footprint of our machines and the process. Having 6K Additive’s titanium sustainable powder added as an approved qualified powder, ensures customers get the quality assurance with the added value of driving down their CO2 footprint.”

Both organisations have a strong customer base in aerospace as well as initiatives toward sustainability.

Frank Roberts, President of 6K Additive added, “We continue to hear from our aerospace and defence customers asking us to help lower the barriers for qualification for their applications. The collaboration between our two companies did just that by ensuring the machine and powder are qualified ahead of their own internal qualification, which will streamline the customer’s process into production faster. We are excited to work with the TRUMPF team on titanium and other powders in our portfolio going forward.”

6K Additive offers a full suite of metal and alloy powders, including nickel, titanium, copper, stainless steel, and refractory metals such as tungsten, niobium, and rhenium. Backed by the UniMElt production-scale microwave plasma process, the technology precisely spheroidizes metal powders while controlling the chemistry and porosity of the final product with zero contamination and high-throughput. An independent LCA study validates that the approach makes it possible to achieve reductions in energy usage and carbon emissions of 90% for its nickel-based alloys and a 75% reduction in titanium alloys.

www.trumpf.com

www.6kinc.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
MaterialsNews
April 2, 2025

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap