CNPC Powder establishes silver powder production line for EV manufacturer

MaterialsNews
February 13, 2025
CNPC Powder has established a production line for the manufacturing of ultra-high quality silver powder for a leading manufacturer of new energy vehicles (Courtesy CNPC)
CNPC Powder has established a production line for the manufacturing of ultra-high quality silver powder for a leading manufacturer of new energy vehicles (Courtesy CNPC)

CNPC Powder, headquartered in Vancouver, Canada, with metal powder production based in Fengyang, Anhui, China, reports it has officially launched a proprietary intelligent production line (Ag-AMP) for the manufacturing of ultra-high quality silver powder, designed and customised for a leading manufacturer of new energy vehicles.

This Ag-AMP has an annual capacity of 30 metric tons, with products tailored for Additive Manufacturing and other advanced applications. Ag-AMP is also scalable to accommodate growth in the EV market and other advanced industries.

Silver, with its unmatched electrical conductivity (6.3×10⁷ S/m), makes it ideal for high-frequency and precision electronic components. Its low-temperature processability prevents thermal damage to substrates, giving it unique advantages in Cold Spray and Binder Jetting Additive Manufacturing technologies.

In Additive Manufacturing, silver powder demonstrates potential in the electronics, new energy and medical sectors, enabling applications such as conductive circuits, 5G/6G radio frequency devices, biosensors and cold spray coatings. This technology is said to excel in creating complex porous or lattice structures to improve thermal management and minimise material waste, a key advantage for cost-sensitive precious metal applications.

CNPC Powder’s innovative production line delivers premium silver powder with:

  • Ultra-high purity (Ag >99.99%)
  • Superior sphericity (>92%)
  • High apparent and tap density
  • Minimal satellite particles and hollow powder
  • Customisable particle sizes: 0-25 μm, 15-45 μm, 45-150 μm

The fully automated Ag-AMP line integrates quality control systems. CNPC Powder notes the following key technological advantages as driving industrial improvements:

  • Digital management: MES system enables full-process traceability from raw materials to finished products
  • Purity assurance: 100,000-class cleanroom guarantees impurity-free production
  • Precision grading: Airflow classification technology achieves particle size distribution CV <15%
  • Customisation: Supports tailored specifications across 0-150 μm particle ranges

Ag-AMP incorporates a number of eco-friendly innovations, such as a closed-loop water cooling system that has a 30% reduction in energy consumption. CNPC Powder’s full life-cycle silver management system achieves a material recovery rate of over 99%, which significantly reduces customers’ precious metal costs, it was stated.

CNPC Powder offers a comprehensive portfolio spanning materials based on aluminium, titanium, iron, nickel, copper and precious metals. These products meet a variety of advanced manufacturing needs in Additive Manufacturing, MIM and cutting-edge technologies. Looking ahead, CNPC Powder intends to sustainably drive innovation in high-end materials, offering customised solutions to accelerate technological progress and industrial transformation around the world.

www.cnpcpowder.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
MaterialsNews
February 13, 2025

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap