Freemelt extends UKAEA partnership with tungsten tiles production scalability

ApplicationsNews
February 10, 2025
The proof-of-concept project target is to demonstrate volume production using Electron Beam Powder Bed Fusion and, in particular, Freemelt’s eMelt machine above (Courtesy Freemelt AB)
The proof-of-concept project target is to demonstrate volume production using Electron Beam Powder Bed Fusion and, in particular, Freemelt’s eMelt machine above (Courtesy Freemelt AB)

Freemelt AB, based in Mölndal, Sweden, has received an order from the UKAEA (United Kingdom Atomic Energy Authority) to conduct production scalability tests of additively manufactured tungsten tiles for fusion energy power plants. The order is expected to be delivered during the first quarter of 2025.

This project is a continuation of previous feasibility studies performed by the two organisations. The proof-of-concept project target is to demonstrate volume production using Electron Beam Powder Bed Fusion (PBF-EB) and, in particular, Freemelt’s eMelt machine .

Freemelt and UKAEA, which have been collaborating since April 2023, have carried out two feasibility studies: the first focused on process development and the second, application testing. In this project, Freemelt intends to demonstrate production scalability of tungsten tiles, a critical step in validating the potential for future volume production. As part of this study, the repeatability of the PBF-EB process will be evaluated to support component qualification programmes for potential use in next-generation fusion energy power plants.

Fusion energy has great potential as energy source, and during the coming years, large experimental tokamaks (experimental fusion reactors using fusion energy) and fusion power plants will require significant volumes of advanced components.

“The fact that we now advance the collaboration to volume production tests of tungsten tiles is an important confirmation that our E-PBF technology meets the demanding requirements in fusion energy,” stated Daniel Gidlund, Freemelt CEO. “Tungsten is one of the most challenging materials to process, and our technology enables the production of complex components with high quality. This is an opportunity to further strengthen our position in the energy sector.”

Unlike today’s nuclear power which relies on fission (nuclear splitting), fusion does not produce long-lived radioactive waste. However, for the process to succeed, extremely high temperatures and advanced materials that can withstand the harsh conditions of the fusion environment are essential.

Test fusion machines like experimental tokamaks are essential for validating fusion technology before scaling to commercial electricity production. They require millions of tungsten components. ITER, the world’s largest experimental tokamak, is predicted to need between 1-1.5 million tungsten tiles, while smaller power plants under development by Tokamak Energy will require about 10% of ITER’s volume.

UKAEA is the UK’s national organisation responsible for fusion energy development and commercialisation, driving several advanced research projects to commercialise fusion as a safe, sustainable, and emissions-free energy source. Through collaborations with industry and academia, UKAEA aims to drive the development of new materials and manufacturing methods required for future fusion power plants.

www.freemelt.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
ApplicationsNews
February 10, 2025

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap