AML3D delivers AM components for testing on US Virginia-class nuclear submarines

ApplicationsNews
January 6, 2025
The prototype tailpiece components have been supplied for testing and in-service trials on board a Virginia-class nuclear submarine (Courtesy US Navel Institute)
The prototype tailpiece components have been supplied for testing and in-service trials on board a Virginia-class nuclear submarine (Courtesy US Navel Institute)

AML3D Limited, headquartered in Edinburgh, Australia, has announced the delivery of a Copper-Nickel component order for the US Navy’s Virginia-class nuclear submarine programme. The prototype tailpiece components, valued at approximately AUS $156,000, have been supplied for testing and in-service trials on board a Virginia-class nuclear submarine. The successful completion of this component order demonstrates how AML3D’s proprietary Additive Manufacturing technology supports the establishment of a resilient trilateral AUKUS supply chain.

AML3D’s advanced Additive Manufacturing technology is delivering a step change in production efficiency and component quality for the US Navy’s Submarine Industrial Base. The Virginia-class submarine prototype tailpiece components were additively manufactured in less than five weeks compared to an average 17-month lead-time via traditional manufacturing. Over the past two years, AML3D has partnered with the US Navy’s Maritime Industrial Base (MIB) Program and BlueForge Alliance to meet emergent material readiness needs for US submarines and integrate metallic Additive Manufacturing as an alternative solution to support critical supply chain gaps and constraints.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

AML3D’s successful delivery of this Virginia-class tailpiece component demonstrates how Australian suppliers are being leveraged to contribute under a tri-lateral industrial base model. AML3D’s contribution to support the AUKUS partnership has been recognised by the Deputy Prime Minister and Minister for Defence Richard Marles, who said, “Production of a US Virginia-class Submarine component in Australia is a great example that AUKUS is happening now, and demonstrates our commitment toward supporting expansion of the trilateral industrial base. Australia’s Nuclear-Powered Submarine Program and the AUKUS partnership will provide incredible opportunities for Australia’s industry, and these opportunities have already started.”

This follows the US Program Executive Office Attack Submarines, Admiral Jonathan Rucker’s noted contribution by AML3D to US Navy efforts. He spoke ahead of the Submarine League Conference in November, revealing he had received an email asking for his formal approval on one of AML3D’s engineering drawings.

“Collaboration in this space is critical to our ability to build and sustain Virginia-class submarines now and for the next many decades. Through partnerships like the one with AML3D, we are creating resiliency and robustness domestically as well as in critical areas of Naval operation,” Admiral Rucker commented.

AML3D CEO Sean Ebert said, “AML3D has been working with the US Navy and its partners for close to two years. In that time, we have created a successful model that includes cross-continental coordination, information sharing, and the deployment of our ARCEMY advanced 3D metal printing technology across a network of US defence industry and academic experts. We have also completed several alloy testing and characterisation programs including Copper-Nickel, which allows us to supply components to the US Nuclear submarine program.”

aml3d.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
ApplicationsNews
January 6, 2025

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap