Research collaboration develops advanced copper Additive Manufacturing process for heat sink design

Additively manufactured component demonstrating grading of pillars which can be used to balance heat transfer and pressure loss of the system (Courtesy University of Wolverhampton)
Additively manufactured component demonstrating grading of pillars which can be used to balance heat transfer and pressure loss of the system (Courtesy University of Wolverhampton)

ToffeeX, London, UK, in collaboration with Imperial College London and the University of Wolverhampton, has developed a design framework that brings multiscale analysis to physics-driven design. At the point of use, this method is said to fully capture thermo-fluid behaviour without the use of computational fluid dynamics (CFD). The University of Wolverhampton has now manufactured the first test specimen created with this method.

Multiscale modelling is reported to offer a computationally efficient solution to the challenges posed by traditional CFD. It models complex systems by solving a series of decoupled smaller systems, which are then assembled to accurately replicate the full behaviour. The decoupling is able to reduce computation time while maintaining high resolution.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

In parallel, the University of Wolverhampton has used its 400 W EOS M290 Laser Beam Powder Bed Fusion (PBF-LB) technology to manufacture these designs in high-purity copper. Known for its high thermal conductivity, copper has traditionally presented challenges in Additive Manufacturing due to its reflective properties. The goal of this partnership was to overcome those obstacles, producing copper heat sinks with enhanced precision and durability, thus showcasing the potential of PBF-LB AM technologies.

Professor Arun Arjunan, director of the university’s Elite Centre for Manufacturing Skills (ECMS) and Centre for Engineering Innovation and Research (CEIR) stated, “Working with ToffeeX, and Imperial College London pushing the boundaries of [PBF-LB] copper printing and heat sink design highlights the potential of Additive Manufacturing and thermal management. By combining our expertise in advanced materials and 3D printing technologies, we will continue to develop innovative solutions that meet the growing demand for efficient thermal management systems across various industries.”

This collaborators have stated that this should mark a significant step forward in both Additive Manufacturing and multiscale modelling, and has a promising future for heat sink design. The collaboration highlights the power of interdisciplinary teamwork to expand technological boundaries.

www.toffeex.com

www.imperial.ac.uk

www.wlv.ac.uk

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap