L3Harris delivers its first additively manufactured copper thrust chamber RL10 rocket engine to ULA

ApplicationsNews
November 26, 2024
The RL10E-1 rocket engine will be used in the ULA Vulcan rocket’s second stage (Courtesy L3Harris Technologies)
The RL10E-1 rocket engine will be used in the ULA Vulcan rocket’s second stage (Courtesy L3Harris Technologies)

L3Harris Technologies, Melbourne, Florida, USA, has delivered the first RL10 engine that features an additively manufactured copper thrust chamber to United Launch Alliance (ULA).

The latest version, the RL10E-1, uses Additive Manufacturing to reduce the number of parts in the thrust chamber by 98%. The engine is set to fly on a ULA Vulcan rocket next year.

The new L3Harris RL10E-1 rocket engine features an additively manufactured copper thrust chamber built with 98% fewer parts than traditional RL10 engines (Courtesy L3Harris Technologies)
The new L3Harris RL10E-1 rocket engine features an additively manufactured copper thrust chamber built with 98% fewer parts than traditional RL10 engines (Courtesy L3Harris Technologies)

“The RL10 has been the nation’s premier high-performance, upper-stage rocket engine for more than 60 years, propelling hundreds of military, civil and commercial satellites into Earth’s orbit and sending spacecraft to explore every planet in our solar system,” stated Kristin Houston, President, Space Propulsion and Power Systems, Aerojet Rocketdyne, L3Harris. “Incorporating 3D printing enables us to build an engine that maintains the performance and reliability our customers have come to expect, while significantly reducing cost and lead time to meet the demands of today’s marketplace.”

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

The RL10 is said to be a highly efficient, upper-stage engine capable of making multiple restarts in space to place spacecraft into precise orbits or propel them to interplanetary destinations. This delivery marks the first of 116 RL10E-1 engines L3Harris will deliver to ULA under its latest contract. Two RL10 engines with a combined thrust of approximately 48,000 pounds will power each Vulcan rocket’s upper stage.

www.l3harris.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

 

 

ApplicationsNews
November 26, 2024

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap