VBN Components has reported that the first in-vitro biocompatibility tests of its additively manufactured Vibenite 350 have been conducted by AM4life (Courtesy VBN Components)
VBN Components has reported that the first in-vitro biocompatibility tests of its additively manufactured Vibenite 350 have been conducted by AM4Life (Courtesy VBN Components)

VBN Components, based in Uppsala, Sweden, has reported that the first in-vitro biocompatibility tests of its additively manufactured Vibenite 350 have been conducted within the competence centre AM4Life. The initial results show that bone-like cells spread and proliferate on the material. These findings are said to further encourage a more in-depth examination of the material’s biocompatibility.

Vibenite 350 is both wear- and corrosion-resistant and could be suited as an implant material where wear resistance is key, such as human joints. It is a cobalt-free material that could replace traditional materials that are not wear-resistant. Additionally, it could be additively manufactured with complex structures adapted to optimise bone cell growth.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

The tests were done at Assistant Professor Gry Hulsart Billström’s Translational Bioprinting Group at Uppsala University, as part of a cooperation with AM4Life Director Professor Cecilia Persson and members of the Tribomaterials Group at Uppsala University, PhD Student Vidhiaza Leviandhika and Professor Urban Wiklund.

The exploration of Vibenite 350 will be continued in the AM4Life competence centre with further biological and tribological tests.

“We are extremely happy of these results and the good cooperation in the AM4life competence centre. When different research fields meet, the greatest results are achieved. But everything relies on good cooperations and the world class science we have in this centre,” said Ulrik Beste, CTO of VBN Components AB.

vbncomponents.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
MaterialsNews
October 21, 2024

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap