Malaysia’s SIRIM receives grant for customised titanium fracture fixation plate implants

ApplicationsNewsResearch
October 11, 2024
Fractures were fully united at week 12. At week 26, the fracture was fully united and a new bone remodelling occurred. Implants remain in-situ
Fractures were fully united at week 12. At week 26, the fracture was fully united and a new bone remodelling occurred. Implants remain in-situ

The Standard and Industrial Research Institute of Malaysia (SIRIM) Berhad has been awarded a grant from The Ministry of Investment, Trade and Industry (MITI) Malaysia to further study a recently developed titanium implant made via Additive Manufacturing.

Developed by team of orthopaedic surgeons, materials scientists, and specialists in precision manufacturing from SIRIM Bhd and the Department of Orthopaedic, Traumatology, and Rehabilitation at the International Islamic University of Malaysia, the has bespoke fracture fixation plate is now undergoing pre-clinical studies and biocompatibility tests.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

Animal implantation studies of additively manufactured Ti6Al4V demonstrates its potential as a viable material for orthopaedic implants. In these studies, the implants showed excellent biocompatibility, successful osseointegration, and increasing mechanical stability over time. Malaysian officials have decided that further studies, including long-term evaluations and clinical trials, are warranted to confirm these findings and facilitate clinical translation.

“The particular advantage of medical implants is that patient-specific, tailored implants offer greater comfort and speedier recovery,” stated Dr Mohammed Afian Omar, the project’s director and Principal Researcher at SIRIM Bhd. “A net-shaped product can be made using the Additive Manufacturing process. It ultimately leads to shorter surgical times due to a particular implant and lower total expenses by modifying the method. Each implant is designed, created, and shipped to the surgeon just before the procedure using just-in-time manufacturing and delivery, removing the need for hospitals to keep a large number of implants in stock.”

The cost of the additively manufactured fracture fixation plates to be studied by the SIRIM Berhad could be decreased by 40-50% in comparison to imported ones. Due to the expense of importing replacement prostheses, Dr Omar stressed the importance of establishing domestic production of bespoke implants.

The industrial research and technology company SIRIM Bhd is owned entirely by the Minister of Finance Incorporated in Malaysia. SIRIM functions as an engine for research and technology development and it has more than forty years of experience.

www.sirim.my

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

 

ApplicationsNewsResearch
October 11, 2024

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap