Tekna offers coarse titanium powders developed for PBF-LB Additive Manufacturing

Tekna Holding ASA, Sherbrooke, Quebec, Canada, reports it is now offering coarse titanium alloy (Ti-6Al-4V) powders for Laser Beam Powder Bed Fusion (PBF-LB) Additive Manufacturing.

The company states that the advancement of PBF-LB machines has opened new possibilities for using larger powder sizes, marking a transformative shift in the market. Addressing this emerging demand, Tekna has developed a range of Ti64 coarse powders specifically engineered for PBF-LB applications. The powders are optimised for use with varying layer thicknesses, including 60 µm, 90 µm, and above.

By leveraging its proprietary plasma atomisation technology, Tekna produces Ti64 powders that are reported to be spherical and free from internal porosity. This results in powders with higher density and flowability, which translates into superior mechanical properties in the final manufactured parts. Consequently, this enhances the end-user production yield and part reliability, the company states.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

Economic and safety advantages

The use of thicker deposition layers leads to reduced production times, which enhances productivity and lowers the end-user overall production costs. This economic advantage, combined with the reduction in powder costs, makes the process more cost-effective. Furthermore, the ability of the end-user to procure Ti64 coarse powders and finer PBF-LB size fractions manufactured from the same dedicated plasma atomisers accelerates the industrial qualification.

From a safety perspective, finer powders commonly used in PBF-LB applications are often classified as flammable. In contrast, Ti64 coarse powders produced by Tekna have a lower sensitivity to oxygen thus reducing risks related to powder handling and recycling as well as costs associated with storage and transport.

“Our commitment to safety is essential, both for users and the environment. Thanks to their reduced reactivity, Ti64 coarse powders are not classified as flammable and are not sensitive to static electricity, making them safer to handle. This also simplifies logistics, allowing for easier transportation and compliance with local storage regulations. Ultimately, these advancements reflect our dedication to delivering high-quality products that prioritise safety and efficiency at every stage,” shared Rémy Pontone, VP Sales & Marketing at Tekna.

Productivity boost

Ti64 coarse powders can significantly improve productivity. Based on recent qualifications performed on well-known manufacturing platforms, the productivity for a given part increased from 123 cm³/hr at a 60 µm layer thickness to 254 cm³/hr at a 90 µm layer thickness. Manufacturing thicker layers provides better energy dissipation, which contributes to fewer deformations. This reduces the number and complexity of part supports required during manufacturing. It, therefore, contributes to decreased post-processing time and costs.

Compliance with industry standards

Parts manufactured using Tekna’s Ti64 coarse powders reportedly fulfil critical industry standards, including B348-21, F3001, and F136. These compliances highlight the quality and reliability of the produced parts.

Comparison between actual values measured on parts manufactured with Tekna’s Ti64 coarse powders and ASTM B348-21, F3001-14, and F136-13 standards:

TeknaB348-21 Standard  Ti64 Alloy Bars and BilletsF136-13 Standard Ti64 Alloy Surgical Implant ApplicationsF3001-14 Standard  Ti64 Alloy Powder Bed Fusion
Ultimate Tensile StrengthVertical Direction
1036 MPa
828 MPa
860 MPa
860 MPa
Yield Strength
Vertical Direction

964 MPa

759 MPa

795 MPa

795 MPa
Elongation After Fracture
Vertical Direction
18.80%

10%

10%

10%

Outlook

Tekna’s development of Ti64 coarse powders marks a significant milestone in the Additive Manufacturing industry. As the market continues to evolve, Tekna remains committed to pioneering innovations that drive economic, safety, and productivity advancements, setting new benchmarks for quality and performance.

www.tekna.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

 

 

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap