Knust-Godwin partners with Continuum Powders for advanced Ni718 recycling in oil and gas industry

An additively manufactured part used in the oil and gas industry (left), transformed through precision machining (centre) to meet exacting specifications. When bulk parts reach end-of-life, their material can now be recycled using Continuum’s proprietary, single-step Greyhound M2P platform, with new, high-quality materials provided back to the manufacturer via the Continuum Powder as a Service (CPaaS). The finished oil and gas component (right) features a specialised coating on the interior diameter to reduce wear and extend operational life (Courtesy Knust-Godwin)
An additively manufactured part used in the oil and gas industry (left), transformed through precision machining (centre) to meet exacting specifications. When bulk parts reach end-of-life, their material can now be recycled using Continuum’s proprietary, single-step Greyhound M2P platform, with new, high-quality materials provided back to the manufacturer via the Continuum Powder as a Service (CPaaS). The finished oil and gas component (right) features a specialised coating on the interior diameter to reduce wear and extend operational life (Courtesy Knust-Godwin)

Continuum Powders, based in Los Gatos, California, USA, has announced that Knust-Godwin, a precision contract manufacturer headquartered in Katy, Texas, USA, has selected it as the exclusive metal powders provider for a project supporting a large oil and gas customer needing to recycle nickel alloy parts.

The oil and gas company had a large amount of Ni718-grade internal products hitting end-of-life and needed a cost-effective means to recycle the parts. The company approached Knust-Godwin, who researched industry offerings to determine the best available solution. An existing Knust-Godwin customer recommended that the firm evaluate Continuum Powders.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

Initially, Knust-Godwin was sceptical of recycled powder, but after multiple mechanical test coupons reportedly showed that Continuum Powders’ products met or exceeded other leading non-sustainable powder suppliers, Continuum Powders was officially selected for the project.

“Continuum is doing things that no other metal powders company can currently do when it comes to complete lifecycle management of consumable metal parts,” stated Rob Higby, chief executive officer of Continuum Powders. “With the incredible advancements we’ve made in converting worn parts into new metal powders, it no longer makes sense to simply scrap those parts and purchase metal powders made from virgin metals.”

Not only was Continuum Powders able to easily recycle end-of-life bulk parts with its proprietary, single-step Greyhound M2P platform, but it also supplied Knust-Godwin with new, high-quality Ni718 through its Continuum Powder as a Service (CPaaS).

Knust-Godwin was then able to manufacture new parts for its customer using a Renishaw RenAM500Q Additive Manufacturing machine. Following this project, Knust-Godwin realised the power of using Continuum’s M2P process for recycling manufacturing by-products like oversized or sieved powder.

“Continuum Powders consecutively proved to have the highest quality powders on the market—equal to or above that of all other manufacturers,” stated Michael Corliss of Knust-Godwin. “When you combine that level of quality with the level of sustainability they offer and their Powder as a Service offering – it makes them our de facto go-to provider.”

www.continuumpowders.com

www.kgsbo.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap