AML3D wins grant to increase deposition rates and efficiency

AML3D’s WAM process combines an electric arc with certified welding wire feedstock to additively manufacture medium to large-scale, free-form parts (Courtesy AML3D)
AML3D’s WAM process combines an electric arc with certified welding wire feedstock to additively manufacture medium to large-scale, free-form parts (Courtesy AML3D)

AML3D Limited has announced an AUD $2.24 million investment to accelerate the company’s ARCEMY Increase Deposition Rates (AIDR) project. The new investment will be funded by an AUD $1.12 million grant from South Australia’s Economic Recovery Fund (ERF), matched by contributions totalling the same value by AML3D.

“The award, from the South Australian Government of the $1.12 million Economic Recovery Fund grant, will facilitate a significant investment to keep AML3D and South Australia at the leading edge of advanced manufacturing,” stated Sean Ebert, AML3D CEO.

With the support of the South Australian Government, AML3D’s accelerated ADIR project will run for a 15-month period, commencing in August 2024, and initially create an additional four highly-skilled, advanced manufacturing and software development jobs. ERF grant payments will be made as reimbursements of eligible project expenses over the course of the project.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

A successful conclusion of the AIDR project will further extend AML3D’s technology and first-mover advantage in both the domestic and international markets and enhance South Australia’s reputation as a globally significant hub for advanced metal manufacturing and technology advances. AML3D is already supporting the commercial adoption of advanced manufacturing, with contracts to supply ARCEMY systems and metal AM components to the Australian and US Defence sectors, including supporting the US Navy’s submarine industrial base.

The AIDR project will reinforce the South Australian and national advanced manufacturing eco-system. Metal AM consumables used in the project will be sourced through South Australian suppliers, with verification testing being carried out in Australia at an approved National Association of Testing Authorities laboratory. A functioning AIDR metal AM machine will have the ability to produce large-scale and exotic material parts even faster, using less energy, creating less waste and to a higher standard than traditional manufacturing process.

“AML3D is proud to be contributing to technology leadership and economic development in South Australia and to be leveraging this on a global scale. From our global base in Adelaide, we are delivering ARCEMY systems and metal 3D printed components to support the US Navy’s submarine industrial base, the Australian Defence and Science Technology Group and tier one, global customers such as Boeing and Chevron,” added Ebert.

Achieving the ADIR end point of a multi-robot, twin wire ARCEMY system has the potential to further revolutionise South Australian and Australian advanced manufacturing by delivering increased productivity, innovation, and global competitiveness. “Having the South Australian Government support the development of the next generation of our ARCEMY technology is expected to keep AML3D and South Australia at the forefront of advanced manufacturing in the years to come,” concluded Ebert.

www.aml3d.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap