Avio produces jet engine titanium turbine blades using high power Electron Beam Melting system

Engineers at the Italian aerospace company Avio Aero, part of the GE Aviation group, have developed a process for Additively Manufacturing light-weight metal blades for jet engine turbines from titanium powder. The method builds the blades from a titanium powder fused with a beam of electrons accelerated by a 3-kilowatt electron gun.

The gun is reported to be ten times more powerful than laser beams currently used for printing metal parts. This boost in power allows Avio to build blades from layers of powder that are more than four times thicker than those used by laser-powered 3D printers.

As a result, one machine can produce eight stage 7 blades for the low pressure turbine that goes inside the GEnx jet engine in just 72 hours.“This is very competitive with casting, which is how we used to make them,” stated Mauro Varetti, advanced manufacturing engineer at Avio.

ge-blades
Avio has 3D printed titanium turbine blades for the LEAP, GEnx, GE90 and GE9X jet engines (Image courtesy GE)

Avio developed the electron beam melting (EBM) technology together with Sweden’s Arcam. The idea was to improve the manufacturing of parts made from an advanced aerospace material titanium aluminide (TiAl). The material is 50% lighter than the nickel-based alloys typically used for low pressure turbine blades.

Blades made from the material can reduce the weight of the entire low pressure turbine by 20%. “Although the material is expensive, the weight savings and the fuel consumption savings tied to weight reduction more than pay for it,” added Varetti. Engineers can also change the shape of the blades and print different blades on the same machine in a quick succession, which would be laborious and expensive with casting processes.

GE will begin testing blades printed for the GEnx engine at its test facility in Peebles, Ohio, later this year. The parts will also go inside the GE9X, a new jet engine GE is developing for Boeing’s next-generation long-haul plane, the 777X.

www.ge.com

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap