Development of customised total hip replacement using Additive Manufacturing
July 3, 2015
A cost effective method of producing customised total hip replacement implants has been developed using Additive Manufacturing technology at Malaysia’s Advanced Materials Research Centre, SIRIM Berhad, reports Dr Mohd Afian Omar ... Read more »