Deutsche Edelstahlwerke offers metal powders for Additive Manufacturing

July 6, 2022

Deutsche Edelstahlwerke offers over 200 grades of powder suitable for Additive Manufacturing (Courtesy Deutsche Edelstahlwerke)
Deutsche Edelstahlwerke offers over 200 grades of powder suitable for Additive Manufacturing (Courtesy Deutsche Edelstahlwerke)

Deutsche Edelstahlwerke, Witten, Germany, now offers a range of gas atomised metal powders for Laser Beam Powder Bed Fusion (PBF-LB) Additive Manufacturing under the brand name Printdur. Available powders include Fe-, Ni- and Co-base metal powders, said to be ideally adapted for the PBF-LB process.

Deutsche Edelstahlwerke has more than 160 years of experience in steel production, and draws on this knowledge to provide support to its customers in determining the parameters necessary for their powders, and testing completed powders to customer specifications using its in-house PBF-LB AM capabilities.

Currently, the company produces over 200 metal powder alloys.

www.dew-stahl.com

Deutsche Edelstahlwerke offers over 200 grades of powder suitable for Additive Manufacturing (Courtesy Deutsche Edelstahlwerke)

In the latest issue of Metal AM magazine

Download PDF
 

Extensive AM industry news coverage, as well as the following exclusive deep-dive articles:

  • Transforming access to medical implants with PrinterPrezz
  • Lessons from 2021’s Olympic bike crash
  • Xerox liquid metal AM
  • Additive Manufacturing for oil, gas and maritime
  • Multi-material metal parts by Powder Bed Fusion
  • Findings from Wohlers Report 2022
  • The challenge of grain size: X-ray powder diffraction analysis of parts made by metal AM

The world of metal AM to your inbox

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Sign up

News from the industry…

    News from the industry…

    Discover our magazine archive…

    The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

    • Reports on visits to leading metal AM part manufacturers and industry suppliers
    • Articles on technology and application trends
    • Information on materials developments
    • Reviews of key technical presentations from the international conference circuit
    • International industry news

    All past issues are available to download as free PDFs or view in your browser.

    Browse the archive

    qweqw

    Looking for AM machines, metal powders or part manufacturing services?

    Discover suppliers of these and more in our comprehensive advertisers’ index and buyer’s guide, available in the back of Metal AM magazine.

    • AM machines
    • Process monitoring & calibration
    • Heat treatment & sintering
    • HIP systems & services
    • Pre- & post-processing technology
    • Powders, powder production and analysis
    • Part manufacturers
    • Consulting, training & market data
    Download PDF
    Share via
    Copy link
    Powered by Social Snap