Netherlands Cancer Institute implants its first AM titanium jaw from M3DT
August 5, 2022
Following four years of research, a 3D printed titanium mandible was successfully implanted by the Antoni van Leeuwenhoek Hospital/Netherlands Cancer Institute (NKI) in a patient with head and neck cancer. ... Read more »