HP and Sandvik collaborate to bring advanced materials to HP’s Metal Jet
November 6, 2023
HP Inc has announced a strategic collaboration with Sweden’s Sandvik AB to bring advanced materials, such as superalloys and 316L stainless steel, to HP’s Metal Jet Additive Manufacturing technology. ... Read more »