Honeywell qualifies 6K Additive’s Ni718 for aerospace Additive Manufacturing
June 3, 2025
6K Additive, a division of 6K, based in North Andover, Massachusetts, USA, has announced that Honeywell Aerospace Technologies has qualified its Nickel Ni718 metal powder for use in the Additive Manufacturing ... Read more »